I had my solution in my tank around 2x weeks, but had to decant it to get the tank welded, rinsed only with water.
The shop welded it, must have water/pressure tested, but after a couple of days since, its either a scum layer over all inside, but whats the best way of getting the residue out?
I had to put the solution back in, as I wanted to clean it again after welding, but only another week, as I want to use the bike next weekend. I think it may not be long enough for the solution to work, whats the time length recommended?
My tip is to use warm to hot water to mix the molasses in, as its hell sticky consistency raw.